High-Resolution Photographic Plates For Holography

Holographic Plate & FilmPhotographic plates for holography are very different from conventional plates and films for photography. First, they tend to be sesitive (sensitized) not to the entire spectrum of white light but only to the area where the laser emits. Second, the resolution of the photographic plates for holography is very high. Below is a list of the photographic plates for holography manufactured by Slavich company.

Fields Of Application

VRP-M High-resolution photoplates for holography are designed to record holograms according to co-directed and counter-directed scheme using a continuous or pulse laser with 530 nm wavelength lasing for the purpose of non-destructive testing of equipment parts, optical data processing, for portrait and moving subjects registration.

PFG-01 High-resolution photoplates for holography are designed to record holograms according to co-directed and counter-directed scheme using a continuous or pulse laser with 633 nm wavelength lasing for the purpose of non-destructive testing of equipment parts, optical data processing, for portrait and moving subjects registration.

PFG-03M High-resolution photoplates for holography are designed to record counter-directed and reflectance holograms.

PFG-03C High-resolution photoplates for holography are designed to record color reflectance holograms.

PFG-04 High-resolution photoplates for holography on dichromated gelatin base are designed to record three-dimensional counter- and co-directed holograms.

Characteristics

Name of IndicesVRP-MPFG-01PFG-03MPFG-03СPFG-04
General Light Sensitivity (S 0,9) unites GOST0,012-0,030
Diffraction efficiency,  %, not less than354070
Diffraction efficiency,  %, not less than
l = 457 and 514 nm
l = 633 nm
40
40
Holographic sensitivity (H) when
exposed by helium-neon laser (l -633nm)
according to co-directed scheme,
when processed with bleaching,
provided getting of diffraction efficiency,
35 %, J/m2, not less than
1,5
Holographic sensitivity when
exposed by helium-neon laser /l -633nm/
according to counter directed scheme,
J/m2, not more than
20
Holographic sensitivity (H) when exposed by
a laser according to counter directed
scheme, provided getting of diffraction
efficiency not less than 30 %, J/m2, not
more than
— for argon laser l = 457 and 514 nm
— for helium-neon laser l = 633 nm
40
40
Holographic sensitivity (H) when exposed by a laser (l = 488 nm) according to counter directed scheme, provided getting of diffraction efficiency 70 %, J/m2, not more than2500
Maximum Density on the characteristic curve, Dmax, B, not less than3,0
Gamma, (g), not less than5,0
Fog Density, (D0), B, not more than0,02
Boundary zone of spectral sensitization, nm, not more than565650680680
Maximum of spectral sensitization, nm525 ± 5625 ± 10635 ± 5525 ± 5
635 ± 5
Resolving Power (R), mm–1, not less than1570
Strength of swollen emulsion layer after chemical photographic processing, H (gram-force), not less than5 (500)4 (400)0,5 (50)0,5 (50)0,5 (50)
Adhesion between emulsion layer and base after chemical photographic processing, conventional classes A-FА-СА-СА-СА-СА-С
Temperature of emulsion layer deformation, °C, not less than5090343434
Metallic silver content, g/m23,0 ± 0,22,6 ± 0,2
3,3 ± 0,1
1,6 ± 0,13,2 ± 0,1
Thickness of photo layer, micrometer6 ± 16 ± 17 ± 110,5 ± 120 ± 2
Antihalation protectionNONONONONO

Main Sizes Of The Photographic Plates (In Mm) As Follows:

50х50, 63х63, 76х76, 102х102, 102х127, 127х127, 90х120, 130х180, 180х240, 240х300, 300х406, 406х609 (on glass base of 2,10mm thickness) in plastic cases and cardboard boxes. According to an agreement between a customer and a manufacturer the photographic plates can be manufactured of other sizes.

Open and process the photographic plates under indirect safe light conditions with using a dark-red light-filter № 107 for VRP-M photographic plates and with using a dark-green light-filter № 170 for PFG-01PFG-03M photographic plates.

Climate conditions for photographic plates usage: temperature of environment is (20 ± 5)оС, relative humidity of air (65 ± 15)оС.

Chemical-Photographic Processing Conditions Of VRP-M Photographic Plates:

Name of the stagesProcessing time, min.Temperature, оC
Development in SM-6 or VRP-M developer 1:52-320,0 ± 0,5
Washing in water2-320,0 ± 0,5
Bleaching in PBU-amidol bleacherto be bleached completely20,0 ± 2,0
Rinsing10-2020,0 ± 0,5
Finishing washing (water with dampener)120,0 ± 0,5
Drying in the open airto be dried out completelyroom temperature

Chemical-Photographic Processing Conditions Of PFG-01 Photographic Plates:

Name of the stagesProcessing time, min.Temperature, оC
Development in SM-6 developer2-320,0 ± 0,5
Washing in water2-320,0 ± 0,5
Bleaching in PBU-amidol bleacherto be bleached completely + 1 min20,0 ± 2,0
Rinsing15 ± 120,0 ± 0,5
Drying in ethanol:
in 50% ethanol
in 75% ethanol
in 96% ethanol
Drying in the open air
2
2
2
to be dried out completely
15-16
15-16
15-16
room temperature

Chemical-Photographic Processing Conditions Of PFG-03M Photographic Plates:

Name of the stagesProcessing time, min.Temperature, оC
Development in GP-3 developer10 ± 120,0 ± 0,5
Washing in water0,5-1,015-20
Fixing3,0 ± 0,118-21
Washing10 ± 110-15
Drying in ethanol:
in 50% ethanol
in 75% ethanol
in 96% ethanol
Drying in the open air
2
2
2
to be dried out completely
15-16
15-16
15-16
room temperature

Chemical-Photographic Processing Conditions Of PFG-03С Photographic Plates:

Name of the stagesProcessing time, min.Temperature, оC
Hardening619,0 ± 0,5
Washing in running waterUp to 119,0 ± 0,5
Development in VRP developer2-419,0 ± 0,5
Washing in waterUp to 119,0 ± 0,5
Bleaching (it is possible in GP 431 bleacher)5-1019,0 ± 0,5
RinsingUp to 119,0 ± 0,5
Stop-bath119,0 ± 0,5
Drying in ethanol:
in 50% ethanol
in 75% ethanol
in 96% ethanol
Drying in the open air
2
2
2
to be dried out completely
15-16
15-16
15-16
room temperature

Chemical-Photographic Processing Conditions Of PFG-04 Photographic Plates:

Name of the stagesProcessing time, min.Temperature, оC
Thermal hardening in a drying electrical cabinet60 ± 5100 ± 2
Swelling in 0.3M triethanolamine solution1,0 ± 0,120 ± 2
Washing in distilled water1,0 ± 0,120 ± 2
Dehydration in water
Solution of isopropyl alcohol
25% solution
50% solution
75% solution
100% isopropyl alcohol
2,0 ± 0,1
2,0 ± 0,1
2,0 ± 0,1
2,0 ± 0,1
20 ± 2
20 ± 2
20 ± 2
20 ± 2
Thermal hardening in a drying cabinet50 ± 5100 ± 2

Guaranteed Shelf Life Of Photographic Plates Is:

VRP-M — 24 months
PFG-01 — 12 months
PFG-03M – from 6 to 9 months depending on the size and package.
PFG-03С — 9 months
PFG-04 — 8 months

If you are interested in purchasing this article, please contact us: e-mail newslavich@gmail.com